Sn63Pb37 | Eutectic Solder Spheres

Harmonization Code : 8001.20 | Unwrought tin: Tin alloys

PMTC Sn63Pb37 Eutectic Solder Spheres Sn63Pb37 Eutectic Solder Spheres Tin-Lead (Pb) Phase Change Diagram

Main features

  • Eutectic Solder Spheres
  • Tin lead
  • For BGA and CSP components

Product Description

LINQALLOY Sn63Pb37 Eutectic Solder Spheres are Tin-Lead eutectic solder spheres for BGA and CSP components used by companies who have not yet made the transition to Lead-free (Pb-free) soldering.

Each jar has a clear label on the lid specifying the solder ball diameter as well as a label on the front identifying the alloy type, the quantity of spheres in the jar, the date of manufacture, and the product lot (or batch) number. This batch number is also tied to a certificate of conformance that is also provided with the solder spheres and ensures the Sn63Pb37 solder spheres meet the following quality criteria:

  • Tin (Sn): 63%
  • Lead (Pb): 37%
  • Melting Temperature (Eutectic): 183°C
  • Sphericity : Within 1.5%

Diameter Tolerance

  • 0.1mm - 0.25mm (100µm - 250µm) : ± 0.0050mm (± 5µm)
  • 0.3mm - 0.45mm (300µm - 450µm) : ± 0.010mm (± 10µm)
  • 0.5mm - 0.89mm (500µm - 890µm) :  ± 0.020mm ( ± 20µm)

Typical Shelf life is 1 year. If Sealed we can guarantee an extension through CoC for one year from the purchase date instead of the mfg date.

Product Family

233058

Alloy: Sn63/Pb37 » 0.100mm (4mil) » 250,000 spheres
1. Select Diameter
2. Select Package Size

Loading pricing…

Product availability
US Shipping in 6 weeks
CA Shipping in 6 weeks
EU Shipping in 6 weeks
Packaging
Unit of measure Jar
Net weight 0.02 kg
Gross weight 0.0275 kg
Dimensions 6 x 6 x 10 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Alloy Composition
Composition of the alloy material
Sn63Pb37
Alloy Type
A metallic element type
Sn63Pb37
Spheroid Tolerance
The allowed % that a solder ball (solder sphere) can divert from being perfectly round and spherical. We take one lot of solder spheres and divide it into 4 smaller lots. Each lot is then checked with advanced visual inspection systems. If even 1 ball is out of spec, the entire batch is scrapped and reworked!
1.5 %

Additional Information

What do I get when I buy Sn63Pb37 Solder Spheres from KRAYDEN?

The advantage of ordering solder spheres online at KRAYDEN.com is that you can be sure of the quality. The solder spheres you receive are originally manufactured solder spheres packed into jars with inert gas (nitrogen). We do not repack the solder balls we receive, so the jars you will receive have never been opened, thus ensuring the quality of the product you receive. The lid of the jar is also always sealed with a shrink-wrapped plastic wrap ensuring that the solder spheres do not oxidate in the jar.

 

Description Popular Brand1
Names
Competitive crossovers 
Tin/Lead (Sn63Pb37) Eutectic Solder Spheres. Products similar to LINQALLOY Sn63Pb37 Solder Spheres
  • Senju Sparkle Ball Sn63Pb37
  • Henkel Accurus Sn63Pb37
  • Nippon Micrometal Sn63Pb37
  • Cookson Alpha Sn63Pb37
  • Indium Precision Spheres Sn63Pb37
  • Kester (EasySpheres) 10-6337
1 Sparkleballs®, Multicore Accurus®, Micrometal®, Precision Spheres®, Alphametal® and Ultra-Spheres® are registered trademarks of Senju, Henkel, NMC, Indium, Cookson and Kester respectively and are not affiliated with this site.

Presentation

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers