DOWSIL 1-2620

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

DOWSIL™ 1-2620 Low VOC Conformal Coating

Main features

  • One-part silicone conformal coating
  • Wide operating temperature range (-45°C to 200°C)
  • UV indicator for inspection and process control

Product Description

DOWSIL™ 1-2620 Low VOC Conformal Coating is a one-part, solvent-borne silicone resin conformal coating designed for protective coating of rigid and flexible circuit boards and PCB system applications. It provides 350 cP viscosity, 80 Shore A hardness, and UV indicator support while supporting room-temperature moisture cure and optional mild heat acceleration after solvent flash-off. This makes it suitable for PCB assemblies requiring low-viscosity flow, dielectric protection, and abrasion-resistant coating performance, subject to application-specific testing and qualification.

Key features

  • One-part silicone resin solution - supplied as a one-part conformal coating with no separate catalyst or hardener mixing step.
  • Low viscosity - 350 cP viscosity supports flow and filling in narrow gaps and spaces on PCB assemblies.
  • Moisture cure - cures at room temperature with a 15 minute tack-free time at 25°C and optional mild heat acceleration after solvent flash-off.
  • Abrasion-resistant surface - cures to a firm elastoplastic coating with 80 Shore A hardness.
  • Inspection support - contains a UV indicator to support visual or automated coating inspection.
  • Recognized coating documentation - listed with UL 94 V-0, UL 746E, IPC-CC-830 Amendment 1, and MIL-I-46058C Amendment 7 in the supplied product data.

Applications

DOWSIL™ 1-2620 Low VOC Conformal Coating is suitable for electronics assemblies where low-viscosity silicone coating, circuit-board protection, and coating inspection are part of the application review.

  • Rigid and flexible circuit boards: suitable for protective coating of printed circuit boards and PCB system applications.
  • PCB assembly protection: supports environmental protection, corrosion resistance, and dielectric protection requirements.
  • Narrow-gap coating areas: low viscosity supports flow and filling in tight spaces and complex board geometries.
  • Thin-section encapsulation: suitable for thin protective coating applications where solvent-borne silicone flow is required.

Related resources

Technical Specifications

General Properties
Color
The color
Translucent
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.88
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
350 mPa.s
Electrical Properties
Dielectric Strength
Dielectric strength is measured in kV per mm and is calculated by the Breakdown voltage divided by the thickness of the tested material. Those two properties go hand in hand and while Breakdown voltage is always thickness dependent, dielectric strength is a general material property. As an example, the dielectric strength of Polyimide is 236 kV/mm. If we place 1mm of Polyimide between two electrodes, it will act as an insulator until the voltage between the electrodes reaches 236 kV. At this point it will start acting as a good conductor, causing sparks, potential punctures and current flow.
16 kV/mm
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
1.05e+15 Ohms⋅cm
Thermal Properties
UL 94 Rating
Flammability rating classification. It determines how fast a material burns or extinguishes once it is ignited. HB: slow burning on a horizontal specimen; burning rate less than 76 mm/min for thickness less than 3 mm or burning stops before 100 mm V-2: burning stops within 30 seconds on a vertical specimen; drips of flaming particles are allowed. V-1: burning stops within 30 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. V-0: burning stops within 10 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. 5VB: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may develop a hole. 5VA: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may not develop a hole
V-0

Additional Information

Conformal coating

DOWSIL™ 1-2620 Low VOC Conformal Coating

DOWSIL™ 1-2620 Low VOC Conformal Coating is a one-part, translucent, low-viscosity silicone resin solution for protective coating of rigid and flexible circuit boards and PCB system applications. It is designed for applications requiring a firm, elastoplastic, abrasion-resistant surface after cure, low-viscosity flow into narrow spaces, UV inspection support, and reduced VOC positioning compared with DOWSIL™ 1-2620 Dispersion.

350 cP viscosity 80 Shore A UV indicator UL 94 V-0 IPC-CC-830 Amendment 1
Conformal Coating for PCBA
Low-VOC silicone conformal coating for PCB assembly protection
Selection fit

Low-viscosity coating with inspection support

  • One-part silicone resin solution for protective circuit-board coating.
  • 350 cP viscosity supports flow and filling in narrow gaps and spaces.
  • Translucent clear cured appearance supports visual review of coated areas.
  • UV indicator supports manual or automated coating inspection.
  • Firm, elastoplastic, abrasion-resistant cured surface with 80 Shore A hardness.
  • Low-VOC version of DOWSIL™ 1-2620 Dispersion.
Processing summary

Room-temperature moisture cure

Number of parts: one-part material.
Cure type: moisture cure at room temperature.
Tack-free time: 15 minutes at 25°C; 5 minutes at 60°C and 15% RH.
Application methods: dip, spray, brush, flow, and automated pattern coating are listed in the supplied data set.
Heat acceleration: mild heat can be used after sufficient solvent flash-off.
Product resources
Product selection

Solvent-based RTV conformal coating selection table

Use this compact comparison to review DOWSIL™ solvent-based RTV conformal coating options by viscosity, non-volatile content, tack-free time, hardness, inspection method, and documented agency listing context. The highlighted row shows where DOWSIL™ 1-2620 Low VOC Conformal Coating fits when reduced-VOC positioning and low-viscosity flow into narrow gaps are part of the application review.

Product and positioning Viscosity / non-volatile content Tack-free time at 25°C Typical hardness Inspection Compliance Selection basis
DOWSIL™ 1-2577 Conformal Coating
Medium-viscosity, firm, abrasion-resistant standard solvent-borne coating
950 cP / 72% 7 min 80 Shore A / 20 Shore D UV indicator UL 94 V-0; UL 746E; IPC-CC-830; MIL-I-46058C Amendment 7 Select when a medium-viscosity, UV-inspectable coating with a firm abrasion-resistant surface is required.
DOWSIL™ 1-2577 Low VOC Conformal Coating
Reduced-VOC, lower-odor version of 1-2577; medium viscosity
1,050 cP / approximately 34% 6 min 85 Shore A / 25 Shore D UV indicator UL 94 V-0; UL 746E; IPC-CC-830 Amendment 1; MIL-I-46058C Amendment 7 Select when the performance profile of 1-2577 is required together with reduced VOC content and lower odor.
DOWSIL™ 1-2620 Dispersion
Low-viscosity standard solvent-borne coating for thinner coating, greater coverage per kilogram, and faster dispensing
150 cP / 59% 5 min 80 Shore A / 25 Shore D UV indicator UL 94 V-0; UL 746E; IPC-CC-830; MIL-I-46058C Amendment 7 Select when very low viscosity, flow, thin coating, material coverage, or dispensing speed is the primary process requirement.
DOWSIL™ 1-2620 Low VOC Conformal Coating
Reduced-VOC, lower-odor version of 1-2620 Dispersion; low viscosity
350 cP / approximately 31% 15 min 80 Shore A UV indicator UL 94 V-0; UL 746E; IPC-CC-830 Amendment 1; MIL-I-46058C Amendment 7 Select when reduced VOC content and enhanced flow into narrow gaps and spaces are required.
DOWSIL™ CC-2570 Conformal Coating
Non-fluorescent, medium-viscosity coating for improved optical performance
1,000 cP / 72% 7 min 76 Shore A / 25 Shore D No fluorescence UL 94 V-0; UL 746E Select when fluorescence must be avoided and a medium-viscosity coating is needed.
DOWSIL™ CC-2571 Conformal Coating
Non-fluorescent, very-low-viscosity coating for improved optical performance
75 cP / 55% 15 min 80 Shore A / 25 Shore D No fluorescence UL 94 V-0; UL 746E Select when fluorescence must be avoided and maximum flow from this product group is required.
Application guidance

Process points to confirm before qualification

Surface condition
  • Apply to clean and dry substrates.
  • Review flux residues, oils, dust, and process contamination before coating.
  • Validate adhesion on the actual PCB laminate, solder mask, metals, and component surfaces.
Coating process
  • Review spray, brush, flow, dip, or automated pattern coating for the actual line.
  • Use the 350 cP viscosity together with target wet-film thickness and keep-out areas.
  • Confirm coating flow around component edges, leads, solder joints, vias, and narrow gaps.
Cure and inspection
  • Allow sufficient solvent flash-off before applying mild heat.
  • Use tack-free time as a handling indicator, not as final property confirmation.
  • Use the UV indicator to support coating-presence inspection, then separately verify film thickness, adhesion, and electrical performance.
Repair and rework
  • Review local coating removal by mechanical means or suitable solvents where appropriate.
  • Clean and dry the affected area before recoating.
  • Confirm repaired-area adhesion and coating continuity before release.
Applications

Where DOWSIL™ 1-2620 Low VOC fits

PCB assembly protection
Suitable for rigid and flexible printed circuit boards and PCB system applications requiring a protective conformal coating. Review actual board design, coating thickness, and operating environment before qualification.
Narrow-gap coverage
350 cP viscosity supports flow and filling in narrow gaps and spaces. Confirm coverage around leads, solder joints, component edges, vias, and keep-out areas on the actual assembly.
Dielectric and environmental protection
Suitable for applications reviewing dielectric protection, corrosion resistance, environmental protection, and thin-section encapsulation with a solvent-borne silicone coating.
FAQ

Frequently asked questions about DOWSIL™ 1-2620 Low VOC Conformal Coating

What is DOWSIL™ 1-2620 Low VOC Conformal Coating used for?

It is used as a protective conformal coating for rigid and flexible circuit boards and PCB system applications, particularly where toughness, abrasion resistance, dielectric protection, and low-viscosity flow are part of the application review.

How does this coating cure?

DOWSIL™ 1-2620 Low VOC cures by atmospheric moisture at room temperature. Mild heat can be used to accelerate processing after sufficient solvent flash-off.

Which application methods are supported?

The supplied data set lists dip, spray, brush, flow, and automated pattern coating. Process fit should be confirmed against the target wet-film thickness, board layout, masking approach, and keep-out areas.

What does the UV indicator confirm?

The UV indicator supports inspection of coating presence. It should not be treated as proof of final dry-film thickness, full cure, adhesion, absence of defects, or long-term electrical reliability.

Is Low VOC the same as solvent-free?

No. DOWSIL™ 1-2620 Low VOC is a solvent-borne silicone resin solution. Review the current SDS before storage, handling, dispensing, curing, cleaning, transport, or waste disposal.

Next steps

Review DOWSIL™ 1-2620 Low VOC for your coating process

Share your board type, coating method, target film thickness, keep-out areas, cure conditions, inspection method, and reliability requirements so the application fit can be reviewed against the available Dow product data.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers